[1]
|
Cattell, M.J., Knowles, J.C., Clarke, R.L. and Lynch, E. (1999) The biaxial flexural strength of two pressable ceramic systems. Journal of Dentistry, 27, 183-196.
doi:10.1016/S0300-5712(98)00047-5
|
[2]
|
Lawn, B.R., Deng, Y. and Thompson, V.P. (2001) Use of contact testing in the characterization and desing of all- ceramic crownlike layer structures. Journal of Prosthetic Dentistry, 86, 495-510. doi:10.1067/mpr.2001.119581
|
[3]
|
Dickerson, W. and Miyasaki, M. (1999) The esthetic revolution continues-IPS Empress. Journal of Oral Health, 2, 87-90.
|
[4]
|
Update technical. (2005) Ivoclar vivadent technical, manufactuer’s production manual. Ivoclar Vivadent.
|
[5]
|
IPS e-max CAD, Lab+to+Dentist (2005)
www.ivoclarvivadent.com, Ivoclar Vivadent.
|
[6]
|
McLaren, E.A. and Terry, D.A. (2002) CAD/CAM sys- tems, materials and clinical guidelines for all-ceramic crowns and fixed partial dentures. Compendium Con- tinuing Education Dentistry, 23, 637-641.
|
[7]
|
White, W.B. (1992) Theory of corrosion of glass and ceramics. In: Clarke, D.E. and Zoitos, B.K., Eds. Cor- rosion of Glass, Ceramics and Superconductors. Noyes Publications, Park Ridge, 2, 2-28.
|
[8]
|
Milleding, P., Wenneberg, A., Alaeddin, S. and Karlesson, S. and Simon, E. (1999) Surface corrosion of dental ceramics in vitro. Biomaterials, 26, 733-746.
doi:10.1016/S0142-9612(98)00223-3
|
[9]
|
Kroeze, H.J., Plasschaert, A.J., Van’t Hof, M.A. and Truin, G.J. (1990) Prevalence and need or replacement of amalgam and composite restoration in Dutch adults. Journal of Dental Research, 69, 1270-1274.
doi:10.1177/00220345900690060901
|
[10]
|
Anusavice, K.J. (1996) Phillips Science of dental materials.10th Edition, WB Saunders Co., Philadelphia.
|
[11]
|
Marx. R. and Fischer, H. (2001) Interner Bericht an Ivoclar Vivadent AG.
|
[12]
|
Albakry, M., Guazzato, M. and Swain, M.V. (2003) Biaxial flexural strength, elastic moduli and x ray diffraction characterization on three pressable all-ceramic materials. The Journal of Prosthetic Dentistry, 89, 374-380. doi:10.1067/mpr.2003.42
|
[13]
|
Albakry, M., Guazzato, M. and Swain, M.V. (2003) Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials. Journal of Dentistry, 31,181-188.
doi:10.1016/S0300-5712(03)00025-3
|
[14]
|
Anusavice, K.J. and Zhang, N.-Z. (1997) Chemical durability of Dicor and Lithia-based glass-ceramics. Dental Materials, 13, 13-19 doi:10.1016/S0109-5641(97)80003-6
|
[15]
|
Sadighpour, L., Geramipanah, F., Raeesi, B. (2006) In vitro mechanical tests for modern dental ceramics. Journal of Dentistry, Tehran University of Medical Sciences, Tehran, 3, 143-152.
|
[16]
|
ISO. (1995) Dental ceramic ISO Standard 6672 - 1995, International organization for Standardization.
|
[17]
|
Marshall, D.B. (1980) An improved biaxial flexure test for ceramics. American Ceramic Society Bulletin, 59, 551-553.
|
[18]
|
Wachtman J.R. Jr, Capps, W. and Mandel, J. (1972) Biaxial flexure tests of ceramic substrates. Journal of Materials, 7, 188-194.
|
[19]
|
Kirstein, A.F. and Woolley, R.M. (1967) Symmetrical bending of thin circular elastic plates of equally spaced point supports. Journal of research of the National Bureau of Standards, 71(C), 1-10.
|
[20]
|
Wassermann, A., Kaiser, M. and Strub, J.R. (2006) Clinical long term results of VITA in-ceram classic crowns and fixed partial dentures: A systematic literature review. International Journal of Prostho- dontics, 19, 355-363.
|
[21]
|
Filser, F., Kocher, P. and Weibel, F. (2001) Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). International Journal of Computerized Dentistry, 4, 89-106.
|
[22]
|
Midelling, P., Haraldsson, C. and Karlsson, S. (2002) Ion leaching from dental ceramics during static in vitro corrosion testing. Journal of Biomedical Materials Research, 61, 541-550. doi:10.1002/jbm.10109
|
[23]
|
Jacobson, N.S., Opila, E.J. and Lee, K.N. (2001) Oxidation and corrosion of ceramics and ceramic matrix composites. Current Opinion in Solid State and Materials Scvience, 5, 301-309.
doi:10.1016/S1359-0286(01)00009-2
|
[24]
|
Hammad, I.A. and Khalil, A.M. (1994) The effect of fluo-ride treatments on glazed and polished ceramic surfaces. Egyptian Dental Journal, 40, 757.
|
[25]
|
Kelly, J.R. (1995) Perspectives on strength. Dental Materials, 11, 103-110.
doi:10.1016/0109-5641(95)80043-3
|
[26]
|
Thompson, G.A. (2004) Determing the slow crack growth parameter and Weibull two-parameter estimates of bilaminate disks by constant displacement-rate flexural testing. Dental Materials, 20, 51-62.
doi:10.1016/S0109-5641(03)00068-X
|
[27]
|
Wagner, W.C. and Chu, T.M. (1996) Biaxial flexural strength and indentation fracture toughness of three new dental core ceramics. The Journal of Prosthetic Dentistry, 76, 140-144. doi:10.1016/S0022-3913(96)90297-8
|
[28]
|
Ban, S. and Anusavice, K.J. (1990) Influence of test method on failure stress of brittle dental materials. Journal of Dental Research, 69, 1791-1799.
doi:10.1177/00220345900690120201
|
[29]
|
Wagner, W.C., O’Brien, W.J. and Mora, G.P. (1992) Fracturesurface analysis of a glaze strenghtened mag- nesia core material. International Journal of Prostho- dontics, 5, 475-478.
|
[30]
|
Craig, R.G. and Powers, J.M. (2002) Restorative dental materials, 11th Edition, Mosby Inc., St Louis.
|
[31]
|
Garcia, C., Galliano, P. and Cerè, S. (2003) Electro- chemical evaluation of resistance to localized corrosion of vitreous coatings containing particles app- lied on metallic substrates for biomedical applications. Materials Letters, 57, 1810-1814.
doi:10.1016/S0167-577X(02)01073-X
|
[32]
|
Grambow, B. (2000) Corrosion of glass. In: Revie, R.W., Ed., Uhlig’s corrosion handbook, 2nd Edition, Wiley, New York, 411-437.
|
[33]
|
Mc Laren, E.A. and White, S.N. (2000) Glass-infiltrated zirconia/alumina-based ceramic for crowns and fixed partial dentures: Clinical and laboratory guidelines. Quin- tenssence Dental Technology, 23, 63-76.
|
[34]
|
Mohsen, S.A. (2004) Corrosion behavior and hardness of veneering materials. Egyptian Dental Journal, 50, 807.
|