[1]
|
M. G. Nicholas and C. F. Old, “Liquid Metal Embrittlement,” Journal of Materials Science, Vol. 14, No. 1, 1979, pp. 1-18. doi:10.1007/BF01028323
|
[2]
|
H. Nies, G. Schambil and B. Stiefel, “The Problems Associated with the Cracking in Hot-Dip-Galvanised Steel Structures,” Welding and Cutting, No. 5, 2007, pp. 256-260.
|
[3]
|
P. Skeldon, J. P. Hilditch, J. R. Hurley and D. R. Tice, “The Liquid Metal Embrittlement of 9Cr Steel in Sodium Environments and the Role of Non-Metallic Impurities,” Corrosion Science, Vol. 36, No. 4, 1994, pp. 593-610.
doi:10.1016/0010-938X(94)90066-3
|
[4]
|
J. P. Hilditch, J. R. Hurley, P. Skeldon and D. R. Tice, “The Liquid Metal Embrittlement of Iron and Ferritic Steels in Sodium,” Corrosion Science, Vol. 37, No. 3, 1995, pp. 445-454. doi:10.1016/0010-938X(95)92861-E
|
[5]
|
O. Hamdane, J. Bouquerel, I. Proriol-Serre and J. B. Vogt, “Effect of Heat Treatment on Liquid Sodium Embrittlement of T91 Martensitic Steel,” Journal of Materials Processing Technology, Vol. 211, No. 12, 2011, 2085-2090.
doi:10.1016/j.jmatprotec.2011.07.006
|
[6]
|
D. Sapundjiev, S. Van Dyck and W. Bojaerts, “Liquid Metal Corrosion of T91 and A316L Materials in Pb-Bi Eutectic at Temperatures 400 -600?C,” Corrosion Science, Vol. 48, No. 3, 2006, pp. 477-594.
doi:10.1016/j.corsci.2005.04.001
|
[7]
|
A. Legris, G. Nicaise, J. B. Vogt, J. Foct, D. Gorse and D. Van?on, “Embrittlement of a Martensitic Steel by Liquid Lead,” Scripta Materialia, Vol. 43, No. 11, 2000, pp. 997-1001. doi:10.1016/S1359-6462(00)00523-6
|
[8]
|
J. Carpio, J. A. Casado, J. A. Alvarez, D. Mendez and F. Gutierrez-Solana, “Stress Corrosion Cracking of Structural Steels Immersed in Hot-Dip Galvanizing Baths,” Engineering Failure Analysis, Vol. 17, No. 1, 2009, pp. 19-27. doi:10.1016/j.engfailanal.2008.11.005
|
[9]
|
J. Carpio, J. A. Casado, J. A. Alvarez and F. Gutierrez-Solana, “Environmental Factors in Failure during Structural Steel Hot-Dip Galvanizing,”Engineering Failure Analysis, Vol. 16, No. 2, 2009, pp. 585-595.
doi:10.1016/j.engfailanal.2008.02.006
|
[10]
|
P. J. L. Fernandes and D. R. H. Jones, “The Effect of Temperature on Fatigue Crack Growth in Liquid Metal Environments,” Corrosion Science, Vol. 38, No. 5, 1996, pp. 745-754. doi:10.1016/0010-938X(95)00163-E
|
[11]
|
Y. J. Su, Y. B. Wang and W. Y Chu, “Chemisorption-Facilitating Dislocation Emission, Multiplication and Motion,” Scripta Materialia, Vol. 36, No. 11, 1997, pp. 1239-1244. doi:10.1016/S1359-6462(97)00020-1
|
[12]
|
B. Donnay, “Failure Mechanisms during Galvanizing,” Proceedings of the European General Galvanizers Association, Edinburgh, 10-14 June 2007.
|
[13]
|
T. Pinger, “Failure Mechanism during Galvanizing (FA-MEGA)—Modelling,” Proceedings of the European General Galvanizers Association, Edinburgh, 10-14 June 2007.
|
[14]
|
A. V?lling, W. Bleck, M. Feldmann and P. Langenberg, “FAMEGA: Laboratory Testing of Zinc Alloys,” Proceedings of the European General Galvanizers Association, Edinburgh, 10-14 June 2007.
|
[15]
|
S. W. Wen and B. Rudd, “Modelling Analysis of Stress and Strain during Hot-Dip Galvanizing,” Proceedings of the European General Galvanizers Association, Edinburgh, 10-14 June 2007.
|
[16]
|
D. Balloy, A.-L. Cristol, C. Niclaeys, P. Quaegebeur and L. Néel, “Experimentation and Modeling of Thermo-Mecanical Phenomena That Appear during Hot Dip Galvanizing,” Proceedings of the International Galvanizing Conference and Exhibition, 22nd, Madrid, 8-12 June 2009.
|
[17]
|
J. Goupy, “Plans D’expériences Pour Surface de Réponse,” In: D. K. G. Roquemore, Technometrics, Vol. 18, 1976, pp. 419-424.
|
[18]
|
K. G. Roquemore, “Hybrid Designs for Quadratic Response Surfaces,” Technometrics, Vol. 18, No. 4, 1976, pp. 419-424. doi:10.1080/00401706.1976.10489473
|
[19]
|
C. Beal, X. Kleber, D. Fabregue and M. Bouzekri, “Embrittlement of a Zinc Coated High Manganese TWIP Steel,” Materials Science and Engineering: A, Vol. 543, 2012, pp. 76-83. doi:10.1016/j.msea.2012.02.049
|
[20]
|
C. Beal, X. Kleber, D. Fabregue and M. Bouzekri, “Liquid Zinc Embrittlement of Twinning-Induced Plasticity Steel,” Scripta Materialia, Vol. 66, No. 12, 2012, 1030-1033. doi:10.1016/j.scriptamat.2011.12.040
|
[21]
|
M. Feldmann, T. Pinger, D. Sh?fer, R. Pope, W. Smith and G. Sedlacek, “Hot-Dip-Zinc-Coating of Prefabricated Structural Steel Components,” Joint Report Number EUR 24286. JRC-ECCS Cooperation Agreement for the Evolution of Eurocode 3, 2010.
|