Electrochemical Deposition and Optimization of Thermoelectric Nanostructured Bismuth Telluride Thick Films

HTML  Download Download as PDF (Size: 2229KB)  PP. 659-667  
DOI: 10.4236/eng.2011.36079    7,194 Downloads   13,427 Views  Citations

Affiliation(s)

.

ABSTRACT

Bismuth telluride thick films are suitable for thermoelectric (TE) devices covering large areas and operating at small-to-moderate temperature differences (20 - 200 K). High efficiency and high coefficient of performance (COP) are expected to be achieved by using thick films in some cooling applications. Bismuth telluride thick films fabrication have been achieved with Galvanostatic and Potentionstatic deposition. Stoichiometric bismuth telluride thick film was obtained by Galvanostatic deposition at current density of 3.1 mAcm-2. Bismuth telluride films with average growth rate of 10 µmh-1 and different composition were obtained. Effects of current density and composition of electrolyte in Galvanostatic deposition were studied. The current density affected the film compactness, where films deposited at lower current density were more compact than those deposited at higher current density. The morphology of the films did not depend on the current density, but chemical composition was observed when different composition of electrolyte was used. Effects of distance between electrodes, composition of electrolyte solution, and stirring in Potentionstatic deposition were studied. The shorter the distance between electrodes, the higher the electric field, thus the higher current density was applied and the deposited film was less compact. The current density increased more rapidly with stirring during electrodeposition which leads to less compact film. Through this study, films electrode-posited from solution containing 0.013 M Bi(NO3)3.5 H2O, 0.01 M TeO2 and 1 M HNO3 at 3.1 mA cm-2 for 6 hours without stirring and with interelectrode distance of 4.5 cm were free-standing with average film thickness of 60 µm and optimum film composition of Bi2Te3. The crystallite size of the later films was found to be around 4.3 nm using Scherrer’s equation from XRD patterns. Also, negative Seebeck coefficient for the same samples was revealed with an average value of -82 μV.K-1.

Share and Cite:

H. Soliman and A. Kashyout, "Electrochemical Deposition and Optimization of Thermoelectric Nanostructured Bismuth Telluride Thick Films," Engineering, Vol. 3 No. 6, 2011, pp. 659-667. doi: 10.4236/eng.2011.36079.

Cited by

[1] electrochemical depoSition of the Sb and Sb-bi nanocryStalline filmS
[2] Thermal transport properties for unveiling the mechanism of BiSbTe alloys in thermoelectric generation: A glance from synchrotron radiation Bi L3-XAFS
Journal of Materials …, 2022
[3] Optical studies on bismuth chalcogenides
2019
[4] Surface Deformation Study of the Electrodeposited Nanostructured Bi2Te3 and Sb2Te3 Thin Films by Double‐Exposure Digital Holographic Interferometry
2019
[5] Electrodeposition of Bi2Te3-based p and n-type ternary thermoelectric compounds in chloride baths
Thin Solid Films, 2018
[6] Electrochemical hydrogen evolution and storage studies on bismuth nano hexagons
International Journal of Hydrogen Energy, 2018
[7] Electrochemical sensor for detection of mercury (II) ions in water using nanostructured bismuth hexagons
Applied Physics A, 2018
[8] Properties of Nanostructure Bismuth Telluride thin films using thermal evaporation
Journal of Nanotechnology, 2017
[9] Fabrication of Microstructured thermoelectric Bi2Te3 thin films by seed layer assisted electrodeposition
Materials Science in Semiconductor Processing, 2016
[10] Fabrication of Microstructured thermoelectric Bi 2 Te 3 thin films by seed layer assisted electrodeposition
Materials Science in Semiconductor Processing, 2016
[11] Effect of different surfactants and thicknesses on electrodeposited films of bismuth telluride and its thermoelectric performance
Materials Research Express, 2015
[12] Fabrication and Optimization of Brush-Printed n-type Bi2Te3 Thick Films for Thermoelectric Cooling Devices
Journal of Electronic Materials, 2015
[13] Structuration de générateurs thermoélectriques sur échangeur de type radiateur par électrodéposition
2015
[14] Growth and Characterization of Silicon Dioxide Thin Films Developed by Anodic Oxidation
2014
[15] Seedless growth of zinc oxide flower-shaped structures on multilayer graphene by electrochemical deposition
Nanoscale research letters, 2014
[16] Growth and Etch Rate Study of Low Temperature Anodic Silicon Dioxide Thin Films
The Scientific World Journal, 2014
[17] Investigation of anodic silicon dioxide thin films for microelectromechanical systems applications
Micro & Nano Letters, 2014
[18] ЭЛЕКТРОХИМИЧЕСКОЕ ОСАЖДЕНИЕ НАНОКРИСТАЛЛИЧЕСКИХ ПЛЕНОК SB И SB-BI
Вестник Тюменского государственного университета, 2013
[19] Effect of Deposition Conditions on the Microstructure and the Thermoelectric Properties of Galvanostatically Electrodeposited Bi
Surface Review and Letters, 2013
[20] Electrodeposition of bismuth, tellurium, and bismuth telluride thin films from choline chloride–oxalic acid ionic liquid
Journal of Applied Electrochemistry, Springer, 2013
[21] Electrodeposition and Thermoelectric Characterization of (00L)-Oriented Bi2Te3 Thin Films on Silicon with Seed Layer
?Journal of Applied Electrochemistry?, 2013
[22] EFFECT OF DEPOSITION CONDITIONS ON THE MICROSTRUCTURE AND THE THERMOELECTRIC PROPERTIES OF GALVANOSTATICALLY ELECTRODEPOSITED Bi2Te …
Surface Review and Letters, 2013
[23] Thermoelectric Thin Film Device of Cross-Plane Configuration Processed by Electrodeposition and Flip-Chip Bonding
Materials Transactions, 2012
[24] Electrochemical deposition of BiTe films from choline chloride–malonic acid mixture as ionic liquid
Chalcogenide Letters, 2012
[25] ELECTROCHEMICAL DEPOSITION OF BITE FILMS FROM CHOLINE CHLORIDEMALONIC ACID MIXTURE AS IONIC LIQUID
2012
[26] Study of High Efficiency Micro Thermoelectric Energy Harvesters
2011

Copyright © 2024 by authors and Scientific Research Publishing Inc.

Creative Commons License

This work and the related PDF file are licensed under a Creative Commons Attribution 4.0 International License.